Resistance Alloy Cr20Ni35

  • Standard

JIS

UNS

EN

ASTM B344

GB/T

NCHW3 / NCHRW3

N08330 / Alloy330

X10NiCrSi35-19 / 1.4886

35Ni-20Cr

Cr20Ni35

  • Description

Cr20Ni35 is an alloy comprising of nickel-iron-chromium with silicon as an additive. Using silicon as an additive gives the alloy enhanced oxidation resistance. This alloy exhibits good strength at high temperatures and good resistance to oxidation and reduction environments. The microstructure of the alloy maintains its stability even after being exposed to high temperatures for long durations.

  • Physical properties

Density (g/cm3)

7.91

Resistivity(μΩ/m)

1.04

Thermal conductivity W/(m.K)

13

Coefficient of thermal expansion 10-6/K

19

Max. Working Temperature ℃

1100

Melting point(℃)

1390

  • Mechanical properties

Tensile strength(Mpa)


Elongation(%)

Elongation(%)

-

Dia. >3.0mm(Wire)

Dia. 0.1-3.0mm(Wire)

-

Thk. > 0.2mm(Strip)

Thk. > 0.2mm(Strip)

min. 600

min . 25

min. 20

  • Application

Industrial heating,Furnaces, muffles, retorts and conveyor systems,heat treating baskets and fixtures.

  • Main customer

1.Amphenol

2.Black+Decker

  • Available Sizes

Thickness:0.1mm-1.5mm

Width:10-250mm

  • Lead time

7-35days

Please contact us for more details about product information, price, packing and shipping.